Not only that, for certain materials like matte and silk I've noticed that i can get good layer adhesion with some temps BUT if im ironing the print, the top ironed layer will look great if i manually reduce the temperature to another setting while its ironing |
Beta Was this translation helpful? Give feedback.
2 replies
Sign up for free
to join this conversation on GitHub.
Already have an account?
Sign in to comment
-
I like to run my BBL X1-Carbon fast
I have the 3rd party nozzle/hotend with 3 holes for better heat transfer to the filament.
So I run a 0.6 mm nozzle, 0.4 mm layers, print temperature @ 135 C for PLA, which is the maximum the heater can provide
It goes fine, but when I add ironing to my print too, I always get heat creep and the filament gets stuck so, I have to take the extruder and nozzle apart to clean out the stuck filament.